Abstract

In this paper, crushed lava granulate was used as full silica sand replacement in composition of repair mortars based on hydrated lime, natural hydraulic lime, or cement-lime binder. Lava granules were analyzed by X-ray fluorescence analysis (XRF), X-ray diffraction (XRD), and scanning electron microscopy (SEM). Particle size distribution of both silica and lava aggregates was assessed using standard sieve analysis. Hygrothermal function of the developed lightweight materials was characterized by the measurement of complete set of hygric, thermal, and structural parameters of the hardened mortar samples that were tested for both 28 days and 90 days cured specimens. As the repair mortars must also meet requirements on mechanical performance, their compressive strength, flexural strength, and dynamic Young’s modulus were tested. The newly developed mortars composed of lava aggregate and hydrated lime or natural hydraulic lime met technical, functional, compatibility, and performance criteria on masonry and rendering materials, and were found well applicable for repair of historically valuable buildings.
In this paper, crushed lava granulate was used as full silica sand replacement in composition of repair mortars based on hydrated lime, natural hydraulic lime, or cement-lime binder. Lava granules were analyzed by X-ray fluorescence analysis (XRF), X-ray diffraction (XRD), and scanning electron microscopy (SEM). Particle size distribution of both silica and lava aggregates was assessed using standard sieve analysis. Hygrothermal function of the developed lightweight materials was characterized by the measurement of complete set of hygric, thermal, and structural parameters of the hardened mortar samples that were tested for both 28 days and 90 days cured specimens. As the repair mortars must also meet requirements on mechanical performance, their compressive strength, flexural strength, and dynamic Young’s modulus were tested. The newly developed mortars composed of lava aggregate and hydrated lime or natural hydraulic lime met technical, functional, compatibility, and performance criteria on masonry and rendering materials, and were found well applicable for repair of historically valuable buildings.

Description

Citation

Materials. 2019, vol. 12, issue 21, p. 1-20.
https://www.mdpi.com/1996-1944/12/21/3557

Document type

Peer-reviewed

Document version

Published version

Date of access to the full text

Language of document

en

Study field

Comittee

Date of acceptance

Defence

Result of defence

Collections

Endorsement

Review

Supplemented By

Referenced By

Creative Commons license

Except where otherwised noted, this item's license is described as Creative Commons Attribution 4.0 International
Citace PRO